The Taber test wears a coated panel under two abrasive wheels for a set number of turns and weighs what is lost. Less weight lost means more wear resistance, but figures only compare when the wheel, load and cycles match.

Abrasion resistance is how well a coating stands up to being worn away. The Taber test puts a number on it by wearing a sample under controlled conditions and weighing the loss.

What the test measures

The test measures the mass of coating removed by a fixed amount of rubbing wear. The result is given in milligrams lost.

How the test is carried out

The Taber abraser is described in several standards, including ASTM D4060, ISO 7784-2 and EN ISO 5470-1. They share one principle.

  • A coated panel is cured, weighed and fixed to a turntable.
  • Two abrasive wheels are lowered onto it under a set load.
  • The turntable rotates for a set number of cycles. The wheels rub a ring into the film.
  • The panel is cleaned and weighed again. The difference is the result.

Three settings decide how severe the test is.

Setting Common choice
Wheel CS-10 or CS-17. CS-17 is the harsher of the two.
Load 1000 g on each wheel.
Cycles 1000.

How to read the result

Lower is better. A coating that loses 40 mg has worn less than one that loses 120 mg in the same test.

A figure is only complete with its conditions, for example "40 mg loss, CS-17 wheels, 1000 g, 1000 cycles". Without them it cannot be compared with anything.

What it means in use

Abrasion is the everyday wear a floor sees: foot traffic, trolley and forklift wheels, and grit carried in on shoes and tyres. A lower loss figure points to a film that keeps its thickness, and its appearance, for longer under that wear.

What the result does not tell you

Results from different wheels, loads or cycle counts cannot be compared. Check the conditions before comparing two products.

The test weighs what is lost. A dense, heavily filled coating can lose more milligrams than a light one while losing no more thickness.

The Taber test is steady rubbing wear. It does not reproduce impact, tyres turning on the spot, or sharp grit being dragged under a pallet. See Impact Resistance and Scratch Resistance for those.

Screed standards use different wear tests and report classes such as AR. An AR class cannot be converted to a Taber figure.

On our product pages

Where a product has been tested, its page shows the result, the method and, where the method has one, the rating. Results published on this site come from internal testing to the stated method. They are given for technical reference and comparison.

If a figure you need is not shown, ask our technical team.

Leave a comment

Please note, comments need to be approved before they are published.

This site is protected by hCaptcha and the hCaptcha Privacy Policy and Terms of Service apply.

Latest Stories

This section doesn’t currently include any content. Add content to this section using the sidebar.