Made In Great Britain

Direct from our factory

Product Test Results

All test results published

Expert Technical Advice

Call or chat with our team

Overview

Overview ⓘ

The falling-weight test drops a weight onto a coated panel from increasing heights until the film cracks or lifts. The result is the largest impact the coating took without damage, as a height and mass or as an energy.

Impact resistance is whether a coating survives a sudden blow. The falling-weight test drops a known weight from a known height and looks for damage.

What the test measures

The test measures a cured film's resistance to cracking, or peeling from the substrate, when it is deformed quickly by a falling weight.

How the test is carried out

The method is ISO 6272. Part 1 uses a large rounded indenter and Part 2 a small one.

  • The coating is applied to a panel and left to cure.
  • The panel is clamped under a vertical guide tube.
  • A weight with a rounded indenter is raised to a set height and released.
  • The area struck is examined for cracks and for film lifting from the panel.
  • The drop height is raised in steps until the film fails.

The test can also be run at one agreed height as a pass or fail.

How to read the result

Higher is better. The result is the greatest drop the coating took without cracking or lifting.

It is reported either as a mass and a height, or as an energy. Impact energy is given in joules or newton metres. They are the same quantity, so 4 J and 4 Nm are equal.

Flooring standards use the same unit. EN 13813 declares impact resistance as an IR class, where the number is the energy in Nm. IR4 means 4 Nm.

What it means in use

Floors and painted equipment take knocks: dropped tools, components, pallets set down hard. A film with good impact resistance deforms and stays whole. A brittle film stars or chips, and the chip is where water and wear get in.

What the result does not tell you

The result is for the coating on its test panel. On a floor, what is underneath matters as much. A coating over weak concrete or a hollow screed can break up under a blow because the surface below it crushed.

A pass means the film did not crack or lift. It does not mean no mark was left. A dent with an unbroken film is still a pass.

Coatings become more brittle in the cold. A result at laboratory temperature does not describe a cold store or a winter yard.

Film thickness changes the result, in either direction. Compare products at the thickness they are applied.

On our product pages

Where a product has been tested, its page shows the result, the method and, where the method has one, the rating. Results published on this site come from internal testing to the stated method. They are given for technical reference and comparison.

If a figure you need is not shown, ask our technical team.

Leave a comment

Please note, comments need to be approved before they are published.

This site is protected by hCaptcha and the hCaptcha Privacy Policy and Terms of Service apply.

Latest Stories

This section doesn’t currently include any content. Add content to this section using the sidebar.